Hey guys, i noticed a few other forums had threads like this so i figured id start one here since i noticed quite a few members enjoy making there own parts like me.

Use this thread to show off your skills/equipment, pictures of things YOU made,talk about processes, and give constructive criticism and tips.

I myself have just picked up a Tig welder and will update in a bit with some of my first welds.

remember fabrication is making just about anything yourself, so post it up!

enjoy.


edit:
first welds on my new machine: hobart 165 ez -tig, 100% argon,60-80 amps on 304 stainless tubing scrap from work, 308 stainless filler rod.





i know that I'm getting it too hot since i've had some practice at work, we use really thin wire there(I'm not sure on the exact measurement), and the thinest i was able to find in stock was 1/16th". to melt the filler into the puddle i have to go slower or else i get the filler stuck to the piece but then it heats up the tubing too much.... i guess it just takes practice, I'm going to try and pick up some thinner filler

heres the best i was able to do, but only for an inch or so..

Last edited by rocknrace03; 05-05-2012 at 10:14 PM.